Friday, October 28, 2011

Re: [MW:12786] flush type

Dear Ali,
             Flush type clean out using for drain the inside liquid completely. Because this elevation will be the same bottom plate elevation. but the nozzles all having some height from the bottom.

L.Venkadesh

On Thu, Oct 27, 2011 at 4:34 PM, Ali Asghari <asghariali@rocketmail.com> wrote:
Dear All
is there a specific meaning for flush type cleanout in API650?
if yes, what is diffrence between it with other nozzles?
Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...