Re: [MW:12770] consumables for welding of SA 516 GR.70 WITH SA 193 GR.B7

Please note that as per ASME section VIII Div 1, it is prohibited to weld a material with more than 0.35% C on a Carbon Steel pressure vessel.
Refer UCS.

Arun

On Sun, Oct 23, 2011 at 10:57 AM, prashant barge <sonupratik2000@gmail.com> wrote:
Dear experts,
 
please suggest me consumables for welding of SA 516 GR.70 WITH SA 193 GR.B7 material.
 
 
regards,
 
prashant
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Arunachalam.A,

Mobile : +971-50-5257122

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...