Re: [MW:12757] May E8018-C1 substitue E8018-G to weld Corten Steel

Yes
 
Spaciicatin is
 WIRE FCAW E 81 T1-W2C/W2C
 availbl from BOHLR
mumtaz
2011/10/22 shrinivas deshpande <shrinivasgundu@yahoo.com>
Dear Experts,
 
Is FCW wire available for welding of Corten steel ? If yes datasheet please !!
 
Shrini
From: Mumtaz Ali Khan <mumtaz.ali662000@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, October 21, 2011 10:08 PM
Subject: Re: [MW:12748] May E8018-C1 substitue E8018-G to weld Corten Steel

Dear
Basicaly Corten is a weather resistance steel only E8018 W2applicable.It is slightly expansive.The chemical composition is totaly different than 8018 c1.If any body want to use 8018 c1 then the purpose of weather resistan will not siolve.

2011/10/20 Zakaria ghrab <zakaria.ghrab@gmail.com>

Hi all

For welding Corten steel, we have in storage E8018-C1 Electrod, may it substitue  E8018-G, how can confirm ?

Regards
--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...