Friday, October 21, 2011

Re: [MW:12746] About welder Qualification as per API 1104

For welder qualification in API 1104,you can use material from any  Group A,B,C
 
Rajesh

--- On Fri, 10/21/11, praneet varma <praneethm14@gmail.com> wrote:

From: praneet varma <praneethm14@gmail.com>
Subject: Re: [MW:12743] About welder Qualification as per API 1104
To: materials-welding@googlegroups.com
Date: Friday, October 21, 2011, 6:23 AM

Dear Mr.harish,
 
You can reffer 5.4.2.2  in  API-1104 ,for Base material gruops As Group-A,Group-B,Group-C.depending up on the yield strength.
 
Thanks&Regards,
 
 
 
 
 
 
 


 
On Sat, Oct 15, 2011 at 1:36 PM, HERISH VARUDE <harish.varude02@gmail.com> wrote:
Dear All Expert ,

I want to know about welder qualification,

If i use API 5L Gr B and API 5L x 52 Gr pipe in one project. Both are different group material As per API 1104 i want both different 

Qualify welding procedure(WPS).But as per API 1104 Base material is not mention.(see 6.2.2 in API 1104)So can i one time qualify 

welder in API 5L Gr B or Gr x 52?will be welder qualify in both WPS?


Remark:

1)Welding Process is same for both wps.

2)Electrode is also same in both wps.

3)Outside dia and thickness is aslo same  in both wps.

4)Only Base material is change in both wps.



So please solve my quarry about it. 

--
Best Regards,

Herish varude
7600046047
(Aneri construction Pvt.Ltd)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...