Hi,
As per Sec.IX,Diameter is not an essential variable. A WPS used for qualification with either  pipe or plate can be qualified to be used for both
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

From: kalyan vvv <vvvkalli@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, October 21, 2011 3:12 PM
Subject: Re: [MW:12740] Welding Process Restriction

There is no diameter limitations in asme sec 9 

On Tue, Jul 26, 2011 at 6:13 AM, Candice Law <candice.law@penergy.com.my> wrote:
 
Expert,
I have a 2 WPS qualified range as below:
1)     WPS A – Qualified Thickness Range from 1.6mm – 11.08mm ; diameter range is all diameter. (Gtaw process)
2)     WPS B – Qualified Thickness Range from 4.8mm – 22.0mm ; diameter range is all diameter. (Gtaw + Smaw process)
Both are qualified under ASME IX and for material with P No.1
 
Now, I need to weld a A106 GrB pipe 4" Sch40, can I use WPS A? Full Gtaw for 4" pipe? Any restriction for welding process pertaining diameter as in ASME IX?
 
Please Advice.
 
Thanks
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
THANKS & REGARDS
 
KALYAN VVV
WELDING ENGINEER
HYDERABAD

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...