Dear
 
First we shuld now the definition of killed and smi killed .In my openion if it is not menioned in MTC bu we can check the chmical composition mainly %of siliconand other deoxidzer element
 
mmtaz

On Wed, Oct 19, 2011 at 3:06 PM, Rajagopal Kannan <rajagopal.kannan@gmail.com> wrote:
Dear All,
I have a query here.In the certification requirements, both in A106 B and A 530 / A 530M, the fully killed statement is not a requirement. If so, Can't we accept a certificate to be deemed as killed, on seeing the certification statement which says the material conforms with the A106 B specification?
Thanks and Regards,
K.Rajagopal

On Tue, Oct 18, 2011 at 3:46 PM, sevak hiren <hirensevak80@gmail.com> wrote:
The mfg TC must show fully killed to comformed the requirement.
 
There are also mfg TC available in market, in which Fully killed / killed is not mentioned, these kind of TCs should not be allowed to use if the requirement is Fully killed.

On Tue, Oct 18, 2011 at 9:45 AM, Vivek Joshi <hifromvivek@gmail.com> wrote:
Hello everybody,
Can somebody tell me please whether ASTM A106 Grade B is fully killed
steel by ASTM specification itself. If not then is it also avalable in
the form of Semi-Killed steel.
Vivek

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards

Hiren Sevak
Surveyor
Bureau Veritas - Ahmedabad
207, Abhishree
Opp Star India Bazaar,
Satellite Road,
Ahmedabad-380015
Tel No. 079-26925491/92


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...