Re: [MW:12712] Re: Accessability of making head from SA516 GR.70

we formed a dished end for our vessel but during hydrotesting some crack were observed, the finding was attributed to flanging process due to it's thickness


From: MOHAMED MOTAWEA <eng.motawea@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Tuesday, 18 October 2011, 16:51:49
Subject: [MW:12711] Re: Accessability of making head from SA516 GR.70

Dear experts,
     Did any body know about the accessibility's of making a head from material SA516 GR.70 with thickness 8mm  . 
So did any body use this with out happening a crack? .
And if any body use it i hope to feed me by a procedure to follow it.
 
Best Regards;
Mohamed  

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...