Tuesday, October 18, 2011

Re: [MW:12708] ASTM A106 Grade B

Hi,
Steel mill manufacturing process and product making process are two different issues, whether hot finished or cold drawn, the original steel stock SHALL be fully killed

--- On Tue, 18/10/11, Karthik <karthik6684@yahoo.com> wrote:

From: Karthik <karthik6684@yahoo.com>
Subject: Re: [MW:12705] ASTM A106 Grade B
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Tuesday, 18 October, 2011, 1:05 PM

Hi,
Yes It shall be Killed steel. But there is an option given in the CODE specificationed as below.
4.3 For pipe NPS 112 [DN 40] and under, it shall be
permissible to furnish hot finished or cold drawn.
4.4 Unless otherwise specified, pipe NPS 2 [DN 50]
and over shall be furnished hot finished. When agreed
upon between the manufacturer and the purchaser, it is
permissible to furnish cold-drawn pipe.
Also find the attached file might be useful to you.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

From: Vivek Joshi <hifromvivek@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Tuesday, October 18, 2011 11:15 AM
Subject: [MW:12702] ASTM A106 Grade B

Hello everybody,
Can somebody tell me please whether ASTM A106 Grade B is fully killed
steel by ASTM specification itself. If not then is it also avalable in
the form of Semi-Killed steel.
Vivek

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...