hai experts ...

  i want to know , how can i propose wps for P11 to SS (TP 321)...with thickness 24.5 mm thickness ... is it require buttering and PWHT,if it have , then how can i do ..?..

once time i have done that first we done butterin on alloy and send to PWHT ... After PWHT we make the joint and done welding ... but here it my client is telling no need PWHT .

IF IT IS NOT DOING PWHT WHAT PROBLEM WILL COME .... AND WHICH FILLER WE CAN USE FOR THIS JOINTS ...

Thanking you ...

NOORUDHEEN P HAMZA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...