Re: Re: [MW:5771] multiprocess qualification(SAW+SMAW)

Mr.Karthi,
Your statement is littlebit confusing for me,pls clarify whether i need to qualify seperate pqr(saw root+smaw outside after backgrinding) or shall i take the support of full saw pqr + full smaw pqr and make new wps alone.

Note:There is no backgrinding in any of these available PQR.
Because SAW ID & OD are welded same time so no backgrinding required for exsisitng wps/pqr,whereas for the new one SAW welded inside & outside we are backgrinding & doing smaw .

regards,
kk
On Mon, 28 Jun 2010 08:50:54 +0530 wrote
>hi,
you can use two wps & pqr...i.e..if you have wps of SAW root and another wps and pqr of SMAW ...So you should have two WPS & PQR as follows..
1.WPS & PQR for SAW only or SAW (root) + SMAW (cover) or any other process
2.WPS and PQR for SMAW or GMAW(root) + SMAW(Cover)
>
Regards,

>
Karthikeyan.S

Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282
>
>--- On Sun, 6/27/10, krishna wrote:
>

>From: krishna
>Subject: [MW:5759] multiprocess qualification(SAW+SMAW)
>To: materials-welding@googlegroups.com
>Date: Sunday, June 27, 2010, 1:13 PM
>
>
Frnds,
>Here our job is welding of spiral pipes by GMAW + SAW.
>Root is continuos tack welded by GMAW & ID & OD WELDED BY SAW.For this we have separate WPS & PQR.
>
>In spiral pipe we have coil joints weld(skelp joints)for that we are doing root & ID welding by SAW but OD welded by SMAW.For this we don't have separate WPS & PQR.Instead we have only SMAW wps/pqr.I mean no multiprocess WPS/PQR.
>
>Now my question is DO we need to qualify a separate PQR for this coil joint(skelp joint welding)i.e SAW + SMAW.
>
>OR is it possible TO prepare a separate WPS taking the support of GMAW + SAW PQR & also SMAW PQR?
>
>Pls tell all your opinion in respect to ASME SEC IX.
>
>THANKS,
>KK
>




--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>












--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...