Re: Re: [MW:5762] API 1104 Code Interpretation

What about 8 inch pipe inclined at 45 degrees?


On Sun, 27 Jun 2010 17:22:24 +0530 wrote
>Hi.


5.4.2.4 Position
A change in position from roll to fixed, or vice versa, constitutes
an essential variable.
For all position is 6G or 5G+2G.

Agustin

>

>


De: limesh M
>Para: Materials & Welding
>Enviado: sáb, junio 26, 2010 5:05:53 AM
>Asunto: [MW:5750] API 1104 Code Interpretation
>
>Dear All,
>
>
>Is position an essential variable in API 1104 ? ie, If a PQR qualified
>on 5G position as per API 1104 qualifies welding on ALL position or
>not?
>
>Thanks and Regards
>
>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>









--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...