Re: [MW:5807] MPI vs DPI

Hi all,
         I have to clarify regarding the MPI that can detect sub-surface. I can't see any code or std mention abt how much depth(6mm) can it detect the defects. Please inform me which std mention may i refer?
 
Thanks & regards,
P.Mahendran

--- On Wed, 30/6/10, manoj john <manojacgnr@gmail.com> wrote:

From: manoj john <manojacgnr@gmail.com>
Subject: Re: [MW:5796] MPI vs DPI
To: materials-welding@googlegroups.com
Date: Wednesday, 30 June, 2010, 8:48 AM

Mpi  can be used only on ferromagnetic materials.  It can detect subsurface defects.
 
DPI can be used on any material.  It can detect only the defects which are open to the surface.

On Tue, Jun 29, 2010 at 5:35 PM, mohammed helal <eng_hilal79@yahoo.com> wrote:
The major difference  is the DPI is only for the defects that open to the surface and the MPI  for the subsurface defect ( 6 mm deep).

Eng.MOHAMMED ABD EL-AZIM HILAL
        MECHANICAL ENGINEER
     CSWIP 3.1 - NDT (RT- MT - PT)
OTISHAN CONSULTANT ENGINEER
 00966-502612218  -  0020103124557


--- On Tue, 6/29/10, george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com> wrote:

From: george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com>
Subject: Re: [MW:5791] MPI vs DPI
To: "materials-welding" <materials-welding@googlegroups.com>
Date: Tuesday, June 29, 2010, 7:06 PM


Mpi  can be used only on ferromagnetic materials


----- Original Message -----
From: Amir Zakee Adnal [amirzakee@gmail.com]
Sent: 29/06/2010 16:52 ZE5
To: materials-welding@googlegroups.com
Subject: [MW:5787] MPI vs DPI



Dear all
What is/are major difference between MPI and DPI? Can MPI be
substitute with DPI? Is there any code or standard that allow such
substitution?

Regards,
Amir Zakee

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...