Re: [MW:5794] MPI vs DPI

The major difference  is the DPI is only for the defects that open to the surface and the MPI  for the subsurface defect ( 6 mm deep).

Eng.MOHAMMED ABD EL-AZIM HILAL
        MECHANICAL ENGINEER
     CSWIP 3.1 - NDT (RT- MT - PT)
OTISHAN CONSULTANT ENGINEER
 00966-502612218  -  0020103124557


--- On Tue, 6/29/10, george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com> wrote:

From: george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com>
Subject: Re: [MW:5791] MPI vs DPI
To: "materials-welding" <materials-welding@googlegroups.com>
Date: Tuesday, June 29, 2010, 7:06 PM

Mpi  can be used only on ferromagnetic materials


----- Original Message -----
From: Amir Zakee Adnal [amirzakee@gmail.com]
Sent: 29/06/2010 16:52 ZE5
To: materials-welding@googlegroups.com
Subject: [MW:5787] MPI vs DPI



Dear all
What is/are major difference between MPI and DPI? Can MPI be
substitute with DPI? Is there any code or standard that allow such
substitution?

Regards,
Amir Zakee

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...