Hi Vijay.
Please read in ASME B16.5 in Table 1B List of Bolting Specifications Applicable ASTM Specifications, the A 320 L7 is high strength and recomended in note 10 : (10) This ferritic material is intended for low temperature service. Use A 194 Gr. 4 or Gr. 7 nuts.
 
Best regards
Agustin Jimenez


De: mahendra reddy <mahendra.mog@gmail.com>
Para: materials-welding@googlegroups.com
Enviado: mar, junio 29, 2010 4:01:41 AM
Asunto: Re: [MW:5780] Fastener Material Regarding

Dear Vijay
 
ASTM A194 Gr.2H IS for high temperature. following list is recommended.
 

Recommended Nuts and Washers

Grade Nuts Washers
L7 A194 Grade 4 or 7 F436
L43 A194 Grade 4 or 7 F436
B8 Class 1 A194 Grade 8 SS304
B8M Class 1 A194 Grade 8M SS316
B8 Class 2 A194 Grade 8, strain hardened SS304
B8M Class 2 A194 Grade 8M, strain hardened SS316

 
 
THX & RGDS
M.M.REDDY
QA/QC INSPECTOR (MECHANICAL)
METHANOL PLANT
DAMIATTA - EGYPT
0020168194532

On Tue, Jun 29, 2010 at 10:14 AM, Vijay <k.vijayaraj@gmail.com> wrote:
Dear All,

For one of our project the fastener requirement was LTCS material as
per project Specification.

The Bolts we received were ASTM A320 Gr. L7 but Nuts we received were
ASTM A194 Gr. 2H

Whether is it is acceptable ????

Kindly clarify.

Regards,
Vijay.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...