Re: [MW:5776] HIC TESTING FOR WELDING

Dear Sachin,
            Please refer TM0284-03 Sec4.2 for HIC testing of welds.

2010/6/29 Kavathekar, Sachin <Sachin.Kavathekar@jacobs.com>

Hi All,

 

Anybody clarify about HIC testing for welding? Which specification we should refer?

Is it required for welding?

 

I know HIC testing for base metal.

 

Regards,

Sachin A Kavathekar.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mahendran p
Sent: Tuesday, June 29, 2010 11:44 AM
To: welding enquiry grp
Subject: [MW:5773] Electrode for 50D material

 

Hi All,

         May any one tell me what is the electrode to be used for 50 D material?

 

Please help.

 

Thank you.

Best Regards,

P.Mahendran

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

NOTICE - This communication may contain confidential and privileged information that is for the sole use of the intended recipient. Any viewing, copying or distribution of, or reliance on this message by unintended recipients is strictly prohibited. If you have received this message in error, please notify us immediately by replying to the message and deleting it from your computer.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



regards,
K Harish Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...