Re: [MW:5761] multiprocess qualification(SAW+SMAW)

Hii,
 
Please check ASME Sec IX ,process is esential variable for PQR or not?If it is essential you have to make new PQR for SMAW + SAW in place of GMAW+SAW
 
I think thickness also taking some serious consideration.
 
Suresh

 
On 6/27/10, krishna <wiqw@rediffmail.com> wrote:
Frnds,
Here our job is welding of spiral pipes by GMAW + SAW.
Root is continuos tack welded by GMAW & ID & OD WELDED BY SAW.For this we have separate WPS & PQR.

In spiral pipe we have coil joints weld(skelp joints)for that we are doing root & ID welding by SAW but OD welded by SMAW.For this we don't have separate WPS & PQR.Instead we have only SMAW wps/pqr.I mean no multiprocess WPS/PQR.

Now my question is DO we need to qualify a separate PQR for this coil joint(skelp joint welding)i.e SAW + SMAW.

OR is it possible TO prepare a separate WPS taking the support of GMAW + SAW PQR & also SMAW PQR?

Pls tell all your opinion in respect to ASME SEC IX.

THANKS,
KK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...