Re: [MW:5756] API 1104 Code Interpretation

Hi.
 

5.4.2.4 Position

A change in position from roll to fixed, or vice versa, constitutes

an essential variable.

For all position is 6G or 5G+2G.

 

Agustin


 


De: limesh M <limesh78@gmail.com>
Para: Materials & Welding <materials-welding@googlegroups.com>
Enviado: sáb, junio 26, 2010 5:05:53 AM
Asunto: [MW:5750] API 1104 Code Interpretation

Dear All,


Is position an essential variable in API 1104 ? ie, If a PQR qualified
on 5G position as per API 1104 qualifies welding on ALL position or
not?

Thanks and Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...