Re: [MW:5740] RE: 5734] welding machine

Hi

Please refer BS 7570 -- code of practice for validation of arc welding equipments.
This standard gives guidance to:
manufacturers about the accuracy required from output meters fitted to the welding equipment and
end users (fabricators) who need to ensure that output meters provide accurate readings.


In short welding machines having output meters can be calibrated by checking the meter reading with a more accurate measuring device and adjusting the readings appropriately.



Regards

Prem Nautiyal

On Fri, 25 Jun 2010 10:48:15 +0530 wrote
>











Tiju



You cannot calibrate a welding power
source – you can only validate the output characteristics.



Use a conventional bench tester to
validate the voltage and amerage characteristics throughout the output curve.



Alternatively use a clamp-on
volt/amperage meter which has been calibrated to validate the output of voltage
and current at specific settings throughout the range of the output curve.







John
du Plessis

Technology Manager



Tel: +27 (11) 298 2100

Tel: +27 (11) 298 2103
(Direct)

Fax: +27 (11) 836 6014

Mobile:+27 (11) 82 883
4970

www.saiw.co.za



This email and any
files transmitted with it are confidential and may be legally privileged. They
are intended solely for the use of the individual or entity to whom they are
addressed. Access to this e-mail by anyone else is unauthorised, and any
disclosure, copying, distribution or other use of this e-mail is prohibited and
may be unlawful. We will not under any circumstances have any responsibility or
liability arising out of or in connection with any unauthorised use of this
e-mail. If you have received this email in error please notify the sender
before deleting it.











From:
materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of tiju koshy

Sent: 24 June 2010 04:24 PM

To:
materials-welding@googlegroups.com

Subject: [MW:5734] welding machine










Hi all,



Can any one advise mehow to calibrate the welding machine.





Regards

Tiju Koshy





--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.









--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...