hi normaly A335 Gr 9 we do purging with argon(100%), we will use ER 80S-B8, preheating requirement is 177 deg c, Pwht requirement is 704-746 deg c, soaking time is -2hrs minimum


From: khadar.M. Rahuman <kmr621212@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wed, 23 June, 2010 1:26:10 AM
Subject: [MW:5723] A335 Gr9

Gents.
 
 
Kindly advice A335 gr 9 material we do PQR...Client advice to Burging ...
 
1. If Burging need where is it mentioned..need to proof evidance.
2.  which electorde . what is the requirment  Pre heat and PWHT requirment..
 


 
Regards.
 
Muzib
QAQC - Incharge .

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...