Hi, pls try welding as AC polarized rod. This will minimize the arc blow.

BR

Bu e-posta, Turkcell BlackBerry ile gönderilmiştir.


From: Muhammed Ibrahim PK <ibratech@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Wed, 23 Jun 2010 13:48:37 +0400
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:5720] How to demagnetise the tube sheet?

Hi Members,
 
We are suffering a problem in tube sheet. The tube sheet is P5A material (SA 336 Gr F22 CL.3) is magnetised.
 
We are not able to proceed the GTAW welding of tube to tube sheet.
 
We are not sure how it is happened. How can we demagnetise the tube sheet.
 
It is around 275 mm Thk and 3 mtr dia.
 
Kindly request the solution from experts.

Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...