Re: [MW:5528] Charpy for A53

The need for impact testing,depends on your client requirement, code of application and MDMT of the service condition, refer to ASME B31.3

Sent from my BlackBerry wireless device from MTN


From: Emilio Cerato <ecerato@hotmail.com>
Sender: materials-welding@googlegroups.com
Date: Thu, 10 Jun 2010 10:43:20 -0300
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:5522] Charpy for A53


Dear All
I need to do a WPS for piping, This pipe drives ammonia.
Is necesary to do impact test?
The material is ASTM A53 GrB
The temperature of operation is -30ºC
I use E7018-1 for weld.
Thanks
 
Emilio Cerato