Hi Tamer.
Check out: APPENDIX E—DIMENSIONS, WEIGHTS, AND TEST PRESSURES—SI UNITS (NORMATIVE)
Tables E-6A, E-6B, and E-6C provide the SI unit values for dimensions, weights per unit length, and test pressures, corresponding
to the U.S. Customary unit values given in Tables 6A, 6B, and 6C.
Table E-6A—Plain-End Line Pipe Dimensions, Weights per Unit Length, and Test Pressures for
Sizes 0.405 Through 1.900 (SI Units)
Agustin Jimenez
De: tamer said <tamer_bajio@yahoo.com>
Para: materials-welding@googlegroups.com
Enviado: lun, junio 7, 2010 4:27:40 AM
Asunto: [MW:5427] Small bore PSL-2 Pipes
Dear all,
Is small bore pipes like 1/2", 3/4", 1" & 2" available in PSL-2 as per API 5L Gr. B or not available.