[MW:5769] RE: 5759] multiprocess qualification(SAW+SMAW)

Dear Krishna,

 

Refer to QW-200.4(a) of ASME Sec. IX, more than one WPS having different essential, supplementary essential or non-essential variables may be used in a single production joint. No need to qualify the multi-process PQR as per above clause.

 

You shall confirm that each WPS shall meet the base metal & weld metal thickness and other variables as required by that welding process need to be considered.

 

Regards,

 

L. Prabhu kumar,

Sr. Principal Engineer,

 

Equipments & Materials Dept.,

Saipem India Projects Limited,

Nungambakkam High Road, Chennai - 600 034, India.

Tel:+91 44 43906588, Ext.: 588, Fax:+91 44 66840345,

Mobile Ph. No.: +91 9003010978.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krishna
Sent: Sunday, June 27, 2010 11:44 AM
To: materials-welding@googlegroups.com
Subject: [MW:5759] multiprocess qualification(SAW+SMAW)

 

Frnds,
Here our job is welding of spiral pipes by GMAW + SAW.
Root is continuos tack welded by GMAW & ID & OD WELDED BY SAW.For this we have separate WPS & PQR.

In spiral pipe we have coil joints weld(skelp joints)for that we are doing root & ID welding by SAW but OD welded by SMAW.For this we don't have separate WPS & PQR.Instead we have only SMAW wps/pqr.I mean no multiprocess WPS/PQR.

Now my question is DO we need to qualify a separate PQR for this coil joint(skelp joint welding)i.e SAW + SMAW.

OR is it possible TO prepare a separate WPS taking the support of GMAW + SAW PQR & also SMAW PQR?

Pls tell all your opinion in respect to ASME SEC IX.

THANKS,
KK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

 




-------------------------------------------------------------------------------------------------------------------------------------------------------------------
DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or 
entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged 
information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution 
or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If 
you have received this communication in error, please notify us immediately by responding to this email and then 
delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete 
transmission of the information contained in this communication nor for any delay in its receipt. 
-------------------------------------------------------------------------------------------------------------------------------------------------------------------

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...