Can any body share the experience in welding of SA240 TP410 Material.

I have a Vessel consists SA387 Gr.11 Cl.2 material cladded with SS410S.

Internal Piping material : SS410S thickness 10-15mm.

Construction Code : ASME SEC VIII Div.1.

Welds in SS410S will under PWHT of low Low alloy steel.

Need guidance in Preheat & interpass temperature of SS410 material welding (Consumable selected for welding of SS410S is 309L type).

regards

P.Rao

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...