Dear all,
 
As per Drawing pipe material is APIL 5L grade X-52 but , can we use ISO -3183-3 L360 MCS material (Thermo Mechanically Treated) which is avilable at site .
 
Both the material is equivalent under Specifed Minimum Yield Strength(SMYS)..But what about other properties like chemical properties etc..will it differ because of heat treatment of pipe during manufacter...
 
Could any one advice on that

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...