Mr. Babu,
The hardness of untempered martensite is determined almost entirely by its carbon content, as shown in the attached diagram.
Regards,
R. W. Warke
Robert W. Warke, P.E.
Associate Professor of
Welding & Materials Joining
School of Engineering & Engineering Technology
LeTourneau University
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Tuesday, June 08, 2010 6:21 AM
To: materials-welding@googlegroups.com
Subject: [MW:5437] Hardness of Untempered Martensite
Hi
Any body have the idea on hardness for the untempered Martensite ?
What will be the morphology of micro?
Thanks & Regards,
K.Babu
Singapore