Hi Jamshed khan,
You must apply as stated in B31.3, 341.3.4.
For example:
A welder did 20 welds, 5% is 1 joint, then,,,
If the first sample is rejected,
2 samples are selected, if rejected 1
2 samples shown again, if rejected 1, evaluate the full lot.
Selected welds were 5, then you from 25% rejection must be evaluated for all welds.
The answer to your question is, rejection is 25%, 50% is greater than what is indicated in the code.
I hope this answers your question.
Kind regards.
Gustavo Mendoza.
QA/QC Inspector.
Venezuela.
mar 13, 2010 03:35:40 AM, materials-welding@googlegroups.com wrote:
===========================================
Hi Friends Let me know in case of excessive repair in Radiography,if RT is 5 % & repair ratio is more then 50 %,then how much pnalty / tracer joints shall be radiographed.?
On Fri, Mar 12, 2010 at 10:13 PM, agmendoza@cantv.net agmendoza@cantv.net> wrote:
Hi, friend
ASME B31.3, do not state anythig about repair twice time on same joint.
Regarding repairs the code state:
341.3.3 Defective Components and Workmanship.
An examined item with one or more defects (imperfections of a type or magnitude exceeding the acceptance criteria of this Code) shall be repaired or replaced; and the new work shall be reexamined by the same methods, to the same extent, and by the same acceptance criteria as required for the original work.
341.3.4 Progressive Sampling for Examination.
When required spot or random examination reveals a defect, then (a) two additional samples of the same kind (if welded or bonded joints, by the same welder, bonder or operator) shall be given the same type of examination
(b) if the items examined as required by (a) above are acceptable, the defective item shall be repaired or replaced and reexamined as specified in para. 341.3.3, and all items represented by these two additional samples shall be accepted, but (c) if any of the items examined as required by (a) above reveals a defect, two further samples of the same kind shall be examined for each defective item found by that sampling (d) if all the items examined as required by (c) above are acceptable, the defective item(s) shall be repaired or replaced and reexamined as specified in para. 341.3.3, and all items represented by the additional sampling shall be accepted, but (e) if any of the items examined as required by (c) above reveals a defect, all items represented by the progressive sampling shall be either
(1) repaired or replaced and reexamined as required, or
(2) fully examined and repaired or replaced as necessary, and reexamined as necessary to meet the requirements of this Code
(f ) If any of the defective items are repaired or replaced, reexamined, and a defect is again detected in the repaired or replaced item, continued progressive sampling in accordance with (a), (c), and (e) is not required based on the defects found in the repair. The defective item(s) shall be repaired or replaced and reexamined until acceptance as specified in para. 341.3.3. Spot or random examination (whichever is applicable) is then performed on the remaining unexamined joints.
I understand the above paragraphs is that the joint should repair again but without tracer.
Kind regards.
Gustavo Mendoza.
QA/QC Inspector.
Venezuela.
mar 12, 2010 03:55:14 AM, materials-welding@googlegroups.com wrote:
===========================================
According to ASME B31.3 ,after NDT if repair twice time on same
joint,what will be procedure as per ASME B 31.3 for tracer joint /
Panely joint
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs
Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-