Wednesday, March 31, 2010

Re: [MW:4651] Multiple PQRs for Impact test requirement

Supporting PQR's qualify the production joint thickness, however check the Base metal group number on PQR, since SA333 Gr6 is Gr1 and SA516 Gr70 falls under Gr2.

WPS should state base metal thickness range as 6-12 and 16-200mm, when impact testing required. and 1.5 to 200mm w/o toughness requirement.

On Wed, Mar 31, 2010 at 7:56 PM, Muhammed Ibrahim <ibratech@gmail.com> wrote:
 
Hi Members,
 
Please provide a solution for the following issue.
 
Shell Material : SA 516 Gr.70 -- 50 mm Thk
Nozzle : SA 333 Gr.6 --- 7 mm thk
 
MDMT : - 46 Deg.C
 
I need to weld the nozzle to shell. I have a PQR with SMAW process qualified in 40 mm thk and another PQR with SMAW qualified in 6 mm thk.
 
As per Sec. IX if impact test is required the 40 mm PQR will support from 16 mm to 200 mm. base metal Thk. and the other PQR will support from 6 mm to 12 mm thk.
 
If I club these PQR can I write a WPS to support 6 mm to 200 mm?.
Is there any issue for the missing range of qualification between 12 mm to 16 mm?.
Or is it required to add another PQR to fill the missing thickness range from 12 to 16 mm between the first two PQRs?.
Or can I write a WPS directly with range 5mm to 200mm omiting impact test requirement for this joint as it is a category D joint and excempted from Production Test Coupon?.

Thanks & Regards
Muhammed Ibrahim PK


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...