Mr. Soliman,
 
The easiest test to determine the correct strength properties (and grade) of the bolts is to perform hardness testing on the cross section of the failed bolts.  The average hardness on the cross section can be converted to an approximate value of ultimate tensile strength (UTS).  If your budget allows, you may also perform a chemical analysis and microstructural analysis, which will tell you if your material is correct and in the proper microstructural condition.  Additionaly, you can have the fracture surfaces of the bolts examined with an SEM that can search for failure mechanisms like hydrogen embrittlement but this is getting more expensive.
 
Regards,
 
Jeremy Zibin, PEng


From: Chandra Bhusan Tripathi <cbt@rediffmail.com>
To: Mohamed.Soliman@WorleyParsons.com
Cc: materials-welding@googlegroups.com
Sent: Tue, March 30, 2010 1:40:52 AM
Subject: Re: [MW:4632] Bolts failure

You can send damaged bolt for tensile testings. Sometime the bolts also fails due to over tightening. Please check with the manufacturer for correct tightening torque.

On Tue, 30 Mar 2010 11:38:16 +0530 wrote
>




Dear all ,

Ihavea casefor the bolts and nutGrade 8.8 ,Carbon steel material according to EN 20 898.Those bolts and nuts are failedduring the tightening and some of the nuts are loose .

What tests can becarried out to ensure the soundness of those bolts .

Best Regards
M.S






Hotmail: Free, trusted and rich email service.
Get it now.


--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at
http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.


--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at
http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.



*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

>
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.


Looking for the perfect gift? Give the gift of Flickr!

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...