Friday, March 26, 2010

Re: [MW:4611] exposure time calculation for CS & SS

Hi Mahendran,
What is the tipe of the chart/table? how to use the table depends on the model or manufacturer
the data normally used are:
Film speed factor in mR/h.
Density required
Distance source-film
Thickness
Source Strength

Kind regards.
Gustavo Mendoza
QA/QC Inspector

mar 25, 2010 11:03:33 AM, materials-welding@googlegroups.com wrote:

===========================================


Hi all,        Can any one help me to send the chart/table for the time calculations of RT using Ir192. I would like to know the time taken depends on the wall thickness & curies.  Regards,P.Mahendran 

     Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...