Hi Mr. Praveen Kumar,
Invite your mail contacts to join your friends list with Windows Live Spaces. It's easy! Try it!
I have tables that are in spanish
in that side there are more data: www.esabna.com/euweb/fm_handbook/577fm8_4.htm
attached as required, I hope is helpful.
Kind regards
Gustavo Mendoza
QA/QC Welding Inspector.
Date: Sat, 20 Mar 2010 13:08:47 +0530
Subject: [MW:4586] Piping welding Electrode Consumption
From: praveenkumar.sek@gmail.com
To: materials-welding@googlegroups.com
               
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
  
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.
 		 	   		  Date: Sat, 20 Mar 2010 13:08:47 +0530
Subject: [MW:4586] Piping welding Electrode Consumption
From: praveenkumar.sek@gmail.com
To: materials-welding@googlegroups.com
Dear all,
 Can anybody give information to me regarding,
 The Exact calculation of Piping welding Electrode Consumption
 (for dia & sch/thkness wise) 
 If any formulas or tables pls assist me 
 Thanks & Regards,
 Praveen Kumar
 --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.
Invite your mail contacts to join your friends list with Windows Live Spaces. It's easy! Try it!
Comments