Monday, March 29, 2010

RE: [MW:4588] Duplex & Superduplex

simply, duplex has 22% Cr, such as Alloy 2205
          super duplex has 25%Cr, such as Alloy 2507.
 
for tube/pipe welding, I recommend GTAW + SMAW process.
GTAW:    AWS A5.9: ER2209        dia. 2.0 or 2.4mm
SMAW:   AWS A5.4: E2209-17   dia. 3.2 or 4.0mm
 
Boehler or Avesta brand is good for your reference!
 
 
Regards
 
Roy
 
 
 
 

Date: Wed, 24 Mar 2010 09:43:00 +0400
Subject: [MW:4601] Duplex & Superduplex
From: ibratech@gmail.com
To: materials-welding@googlegroups.com

Hi friends,
 
How can we identify duplex and super duplex stainless steel?. Both are P10H.
What are the common elcetrodes for Duplex and super duplex?.

Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.


搜索本应是彩色的,快来体验新一代搜索引擎-必应,精美图片每天换哦! 立即试用!

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...