hi all,
         I'm encountering an interesting sfor hardness and impact toughness ituation. My WPS  progression is as follows

 RP-up, Hot- up, fill & cap  - downhill.

(dia-36" No of welders =2,Mat=API 5LX70, code = api1104,toughness and hardess requirements)

Now after root pass due to some unavoidable conditions the pipe has been rotated 90 degrees (12 o clock rotated to 3 o clock). Now considering one half

section of the pipe half portion is welded uphill with one welder and half downhill with the other welder

a) What should be the progression of next pass
b) How the welders must be allocated
c) What area (if required) must be selected for hardness and impact toughness testing.

hope the experts will comment



Sreejith Nair
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...