Re: [MW:4570] Fiber elongation of dish heads

it is knuckle radius plus half the thickness

On 3/15/10, qaqcmpm <mamujeebali@gmail.com> wrote:
> How to calculate the fiber elongation of dish heads as per UCS 79?
> what is Rf final centerline radius & Ro original centerline radius
> (equals infinity for flat
> plate)? Is it crown/spherical radius & knuckle radius respectively?
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
ARUNACHALAM.A
050-5257122

There are three types of people in the world,
First makes wonder happen,
Second see wonders happen and
Third one wonders what happened!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...