Hi Sachin,
The percentage dilution can be determined by measuring areas labeled A and B. Percentage dilution is then calculated as state in figure 1.(attached)
Dilution is usually considered as a percentage of the base metal which has entered into the weld metal.
When two pieces of base metal are welded together, the final composition of the weld deposit consists of a mixture of base metal and filler metal. The portion of the base metal that has been melted in with the filler material and has diluted it may be expressed in percen dilution.
I hope this can help.
Best regards,,
Gustavo Mendoza.
QA/QC Inspector
Venezuela.
mar 13, 2010 04:44:44 AM, materials-welding@googlegroups.com wrote:
===========================================
Hi,
Is their any theoritical formaula to calculate percentage dilution of weld in base metal during cladding
Regards
Sachin
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment