Skip to main content

Re: [MW:4557] Test Specimen Heat Treatment

Hi ,
 
It stated you should hold the Speciment minimum at 80 % of the Maximum Vessel Portion Temp For condition A  ( This information you will get from the Data sheet which give the max exposure of the vessel ) i.e if the Max Vessel Temp is 100 Dec C you should hold the specimen minimum at 80 Degree C and the range can be ( 80 to 100 Degree C )
 
Same for the minimum Temp , the holding Temp for condition B should be minimum 120 % of the Minimum Vessel Temp . i.e if the Minimum Temp is - 40 you should hold at - 48 Deg and the range will be  ( - 40 to - 48 Deg C )
 
Thanks
 
Sujeet

On Mon, Mar 8, 2010 at 12:19 PM, qaqcmpm <mamujeebali@gmail.com> wrote:
3.4.3 Test Specimen Heat Treatment
3.4.3.1 Two sets of tension specimens and one set of Charpy impact
specimens shall be tested. One set each of the tension specimens shall
be exposed to heat treatment condition A. The second set of tension
specimens and the set of Charpy specimens shall be exposed to heat
treatment Condition B.
a) Condition A – ....... Time at temperature shall be no less than 80%
of the actual holding time of the vessel portion exposed to the
maximum vessel-portion temperature.
b) Condition B – ....... Time at temperature shall be no more than
120% of the actual hold time of the vessel portion exposed to the
minimum vessel-portion temperature

Can anybody explain this 80% & 120% with simple example?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...