Wednesday, March 24, 2010

[MW:4603] Code limit of porosity and penetration as per SEC. IX of ASME

Dear All
Good Day
 
What is the code limit (Only Visual Examination) of Porosity and Root Penetration as per SEC. IX of ASME on 6"dia Sch 80(10.97mm thk) pipe Welded by SMAW Process in 6G position(Welder Performance Qualification).
 
As per QW-194 Performance test coupons shall show complete joint penetration with complete fusion of weld metal and base metal.....
 
Kindly Clarify and give ur views on this...
 
RGDS
M.R.Gupta
9820604076


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...