[MW:4585] Re: EN10204 3.2 certification

Dear Arpee,

3.2 certificates can only be drawn up by the original manufacturer of
the material. For this the company needs to have a certief quality
system and always the involvement of a notified body is required. It's
not allowed to draw up your own 3.2 certificates also not when a
customers representative is involved.
What a company has to do when he wants to cut 3.2 certified material
in pieces or wants to machine by which the original marks will be
removed is to re-mark all the seperate parts in front of cutting or
machining with a traceble identification to the original 3.2
certificate (if possible similar marks as on the original material)
and he has to invite a authorized body to put their mark near the re-
stamping in front of cutting in pieces and/or machining. Some
manufacturers have a re-mark approval from a notified body by which
they may re-stamp the material without involvement of this notified
body, they have to show this written approval if you are not sure.
Afterwards the manufacturer always has to draw up a so called re-stamp
declaration in which he mention how may parts with which dimension
where made from the original material, in this declaration they also
have to mention the original and new marks as well as the original
certificate number.

Hope this will help you out.

Best Regards,

Herman Pieper

On 18 mrt, 07:53, Aarpee <ramprasad.ch...@gmail.com> wrote:
> Dear all,
> My understanding about 3.2 certification is that only a 'component'
> manufacturer can issue it with due endorsement by customer's
> represenattive/customer's authorised representative.
> CAN:
> 1 A pressure vessel manufacturer, who does only welding,NDT,Hydro
> etc,issue 3.2 certificate??(he does this from components like
> plates,pipes,flanges,fittings,fasteners,gaskets etc which can be
> either in 3.1 certification or 3.2 certification)
>
> 2.A Piping Skid manufacturer and assembler, who also does
> welding,NDT,Hydro,assembly,pneu test etc,issue a 3.2 certificate??(he
> does this from components like
> pipes,flanges,fittings,fasteners,gaskets,valves,meters,gauges,instruments,c­ables
> etc which can be either with 3.1 certification or 3.2 certification)
>
> Your input with experience on above shall be appreciated.
> Regards
> Aarpee

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...