[MW:4582] corrosion problem in TP321 pipes after hydrotesting

Hi,
We have a 2"Sch-40 A312TP321 piping .We tested the above line 4 months before partially and accepted. Same line when we tested again now it started leaking at several locations(welds and pipe)We tested the water used for testing the line and found that the chloride content is 120ppm
Is it possible that just because of this high chloride content the line starts leaking within 3 months?
 
best regards,
BIJU

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...