Dear Mr. Sachin,

If PQR is qualified in 40mm thick plate or weld metal depositon, Your
WPS is qualified to deposite weld metal up to 200mm, If your repair
job is 300mm but you want to repair it up to depth of 80mm you can.

Similarly if WPS is wualified without backing it is also get
On Mar 10, 8:02 pm, "sachin sankhe" <sachin.san...@rediffmail.com>
wrote:
> Dear Freinds
>
> I have query on casting repair
>
> MOC -SA217 WC9
> THk -200 mm & 300MM
> Repair depth -60 mm & 80mm
>
> Vendor has submitted PQR for butt joint with 40mm thk
> As per ASME sec IX THK QUALIFIED IS 5 MM to 200mm
> So PQR can be used to repair 200 mm base metal having defect of 60mm
> However same PQR cannot be used to repair 300mm base metal with 80 mm depth defect
> Kindly let me know if my understanding on ASME sec IX is correct
>
> Regards
> Sachin

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...