Tuesday, March 23, 2010

FW: [MW:4593] Alloy 20 in DI Water service



Hi Satish,

 

If the deionized water treatment plant involves use of  any form of Sufuric Acid, then 20Cb-3 would be a very reliable material. This material is high alloyed austenitic stainless steel, and surpasses the corrosion resistances of conventional 300 grades(e.g 304/316/321/347…. etc) of  austenitic stainless steels. The corrosion resistances implies to general corrosion, resistance to intergranular corrosion and SCC.

 

Weldability of this alloy is good , but keeping a good control on weld cleanliness would ensure excellent quality of welds.

 

You may find the attached information quite useful.

 

Thanks

 

Pradip Goswami,P.Eng

Senior Engineer/Specialist(Welding-Metallurgy)

Machine Dynamics & Component Integrity Dept.

Engineering & Training Services Division

ONTARIO POWER GENERATION Inc.

34 Regional Road 55, Nanticoke, Ontario,N0A1L0

Tel:-(519) 587-2201, Ext 3107--in Nanticoke

         (416) 231-4111, Ext 5925--in Kipling,Toronto

Fax: (519) 587-6825

Email-pradip.goswami@opg.com.

 

From: sifuentes26@hotmail.com
To: materials-welding@googlegroups.com
Subject: RE: [MW:4580] Alloy 20 in DI Water service
Date: Thu, 18 Mar 2010 16:47:22 -0500

Alloy 20 is compatible to deionized water, check the attached guide on Water Deionized row.
I hope you find the proper information.
                                                Regards
                                                  JRS
 
> Date: Thu, 18 Mar 2010 12:29:12 +0530
> Subject: [MW:4578] Alloy 20 in DI Water service
> From: e1500603@gmail.com
> To: materials-welding@googlegroups.com
>
> Hi
>
> can Alloy 20 (3-4% Cu) be used in De Ionised Water ??
> anbody used this combination ?
>
> Thanks
>
> Satish.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Hotmail has tools for the New Busy. Search, chat and e-mail from your inbox. Learn More.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
To unsubscribe from this group, send email to materials-welding+unsubscribegooglegroups.com or reply to this email with the words "REMOVE ME" as the subject.



THIS MESSAGE IS ONLY INTENDED FOR THE USE OF THE INTENDED RECIPIENT(S) AND MAY CONTAIN INFORMATION THAT IS PRIVILEGED, PROPRIETARY AND/OR CONFIDENTIAL. If you are not the intended recipient, you are hereby notified that any review, retransmission, dissemination, distribution, copying, conversion to hard copy or other use of this communication is strictly prohibited. If you are not the intended recipient and have received this message in error, please notify me by return e-mail and delete this message from your system. Ontario Power Generation Inc.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...