Corrosion in raw steel plates can be evaluated against ISO 8501-1, Preparation of steel substrates before application of paints and related products - Visual assessment of surface cleanliness - Part 1: Rust grades and preparation grades of uncoated steel substrates and of steel substrates after overall removal of previous coatings
 
As far as I remember there is 3 classes of rust grades given here.
 
regards
Kristian


From: sachin sankhe [mailto:sachin.sankhe@rediffmail.com]
Sent: 20. november 2009 18:18
To: materials-welding@googlegroups.com
Subject: Fw: Re: [MW:3706] Re: Tolerance for Pitting of plates

Note: Forwarded message attached

-- Original Message --

From: "sachin sankhe"sachin.sankhe@rediffmail.com
To: mn.senthilkumar@ymail.com
Subject: Re: [MW:3693] Re: Tolerance for Pitting of plates

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...