Re: [MW:3765] Torque calculation

Torque,in lb.ft=KDP/12
 
K=0.2 for finished bolts;0.22 for Zn Plated;0.3 for black;0.16 for Cd plated;0.15 to 0.18 for lubricated;0.10 for highly lubricated or waxed

D=nominal dia of bolt in inches
P=Bolt's desired load in Lbs(=75% of YSXArea)
A,area=0.7854X Square of (D - 0.9743/n)
n=no of threads pre inch;
Coarse series(UNC) 1/2=13
                              5/8=11
                              3/4=10
                              7/8=09
8UN series 1" onwards=8
Hope above information shall help
Regards
Aarpee
On Sun, Nov 29, 2009 at 11:45 AM, Mrityunjay Kumar / ZS Saudi PEB QA/QC <Mrityunjaykumar@zamilsteel.com> wrote:

Hi,

Good morning,

Can anybody tell me the formulae for Torque calculation (if load & area is provided for Anchor Bolts).

 

 

 Thanks and Regards,

M.K.Choudhary

--------------------------------------------------------------------------------------------------------
Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use, disseminate,
distribute, copy or alter this email. Any views or opinions presented in this
email are solely those of the author and might not represent those of "Zamil
Industrial" and or its units.

Warning: Although reasonable precautions have been taken to ensure no viruses
are present in this email, the company cannot accept responsibility for any
loss or damage arising from the use of this email or attachments. If you have
received this electronic mail message in error, please contact the sender directly.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...