Hi!KC
use the following process:for qlfn of pqr
GTAW (root) :ER 80S-Ni1
SMAW :E7018-G

PWHT as per UCS-56 ASME Sec VIII Div 1

After qulaification of PQR & WPS FOLLOW ug-84 for PTC requirements
Rgds
VG



On Thu, Nov 26, 2009 at 4:02 PM, KC <kc.chavda07@gmail.com> wrote:
Can anyone tell me  to weld  the below material with SMAW  which
electrodes we have to use , to weld with SAW which filler wire & flux
combination we have to use.
The material and test requirement is as below…

       Material is SA-537 Class 1, Fully Killed, Normalized, Charpy V-
Impact Tested
       Material is SA-516 Gr.70, Fully Killed, Normalized
       Thickness varies from 38 mm to 50 mm for both materials.
After complication of welding we have to test PTC (production test
coupon) @ -48˚C (Negative 48). The impact energy value shell be 50
joule.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...