Hi!
Prashant
Please wash the steel surface & blast to obtain the required surface roughness.
Then do salt test using Bressel's kit(it cost roughly 2000 dhirams).
Thanks & Rgds
Vg
-- Prashant
Please wash the steel surface & blast to obtain the required surface roughness.
Then do salt test using Bressel's kit(it cost roughly 2000 dhirams).
Thanks & Rgds
Vg
On Wed, Nov 25, 2009 at 12:04 PM, Qamlr <qamlr@cicb-chemicon.com> wrote:
--Dear All
Request your suggestions as to how we can carry out the salt contamination test on job before blasting.. If the salt is > 7 micro gram/cm, then we have to clean the entire surface with water jet .This is recommeded by our client as our manufacturing facility is close to coast.
Thanks & regards
Prashanth Hegde
Head Quality
CICB-Chemicon Pvt. Ltd
Mangalore- INDIA
Please don't print this e-mail unless you really need to.
*******************************************************************
This e-mail is confidential. It may also be legally privileged. If you are not the addressee you may not copy, forward, disclose or use any part of it. If you have received this message in error, please delete it and all copies from your system and notify the sender immediately by return e-mail. Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.
*******************************************************************
"SAVE PAPER - THINK BEFORE YOU PRINT!"
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments