Wednesday, November 25, 2009

Re: [MW:3747] NDT procedure qualification

Hrishi

To make it simple . ASME had introduced mandatory Procedures
Qualifications for NDE in 2007 . These will have Essential variables
akin to WPS in Welding

Although Industry still did not get into this groove

you may find the same in clauses referred by Pradip


Regards

Satish Kumar

On 11/24/09, K.M Hrishikesan <hrishikm07@gmail.com> wrote:
> Is it mandatory to demonstrate NDT procedure qualification before
> applying in the actual job? If so, please give the code/standard reference.
>
> Regards
> Hrishi
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...