Wednesday, November 25, 2009

Re: [MW:3746] NDT procedure qualification

Mr Hrishi,

Please refer ASME Sec V T-150 which is self explainatory, I trust this clarifies ur queiry

Regards,

S A Naik
ASNT Level-III (UT,RT,MT,PT,VT)
API- 570, 510, 653 Certified Inspector
ABS Group INC
Dubai

On Tue, 24 Nov 2009 18:59:16 +0530 wrote
>Is it mandatory to demonstrate NDT procedure qualification before applying in the actual job? If so, please give the code/standard reference.
 
Regards
Hrishi



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...