Re: [MW:3716] scope of ISO Recommendations for Boiler Construction...

Drar Rahul

While designing pipeline you can consider the values given in ASME Se. II part D, table 1A,
as same values are also considered in designing neck thickness of a nozzle, which normally is made from a pipe.

Regards
nspandit

On Fri, Nov 20, 2009 at 3:42 PM, Pisat, R. R(ahul) <Rahul.Pisat@akzonobel.com> wrote:

Hello all,

I have query regarding application A106 specification.

In the old edition of Astm A106 - edition 99 and  latest SA106 specification, there is a clause for Additional requirements of yield strength as per A 520 shall be followed in case the product to be used in application confirming to  ISO recommendations of Boiler Construction.

1 )Can anyone explain me the definition / scope of  ISO recommendations of Boiler construction ?

also. As per current ASTM revisions,  standard A520 has made Obsolete &  the clause of additional requirements for ISO recommended Boiler construction has been removed in revised edition of A106 - edition. 2009.

now to design pipe class according to ASME 31.3 , do I have to consider any additional requirement ?

One of the reply from Lloyds NOBO. was to follow yield strength  as per ASME section II part D table Y-1.

Then for calculations , which allowable stress value shall be consider , ASME 31.3 table A-1  or  ASME Se. II part D, table 1A ?

kindly advise me on the matter.


Kind regards

Rahul

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...