Hi Nimesh

In the past we had welded some galvanised pipes with SMAW - E7018.
However the thickness of your sheets are very less and cant be welded by SMAW.
I recollect that we had also welded some components with TIG - ER70S2. Give it a try with 1.2 mm dia. filler wire and very low amps like 50-70A.

Regards

Prem Nautiyal

On Wed, 18 Nov 2009 21:34:32 +0530 wrote
>Dear All,

Welding of Galvanized Sheets from 1.0mm to 1.5mm

Which is the best process to use ? Arc / TIG / MIG

What should be the parameters ?

Regards,

--
Nimesh S Chinoy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...