Thursday, November 12, 2009

[MW:3638] Stud weld PQR

Dear All

We did a PQR for stud weld according to ASME sec IX & our test passed all except that in micrographic check one of five stud have the discontinuity in the weld. So can any one suggest what we should to do in this case? Repeat the Whole PQR or retest only one piece or etc. unfortunately I didn’t find any explanation in code in this regard.

 

Sincerely yours

 

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...